ESAB

OXWELD Powder Dispenser

Specifications

2217290

Nitrogen Flow 50-200 cfh
Nitrogen Inlet 50 psig
Operating Pressure 5-40 psig
Powder Capacity 100 lb (45 kg)
Powder Flow 15-100 lb/h (7-45 kg/h)
Relief Pressure 45 psig
Type Manual

2223093

Nitrogen Flow 50-200 cfh
Nitrogen Inlet 50 psig
Operating Pressure 5-40 psig
Powder Capacity 181 kg (400 lb)
Powder Flow 15-100 lb/h (7-45 kg/h)
Relief Pressure 45 psig
Type Manual

2220388

Nitrogen Flow 50-200 cfh
Nitrogen Inlet 50 psig
Operating Pressure 5-40 psig
Powder Capacity 181 kg (400 lb)
Powder Flow 15-100 lb/h (7-45 kg/h)
Relief Pressure 45 psig
Type Automatic