This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

OXWELD Powder Dispenser

OXWELD Powder Dispenser

3 legged powder dispenser is the necessary device for proper powder storage and delivery during this process; Keeps the powder dry with no moisture allowed near it at any point.

Where To Buy


Features

  • Heavy welded steel construction
  • Hinged lid with heavy-duty closures
  • Inlet gas filter and moisture trap
  • Pop-off safety valve
  • Screen filter sifts out lumps of powder
  • Manual and automatic models

Industries

  • Industrial and General Fabrication

Specifications

Specifications

2217290

Nitrogen Flow 50-200 cfh
Nitrogen Inlet 50 psig
Operating Pressure 5-40 psig
Powder Capacity 100 lb (45 kg)
Powder Flow 15-100 lb/h (7-45 kg/h)
Relief Pressure 45 psig
Type Manual

2223093

Nitrogen Flow 50-200 cfh
Nitrogen Inlet 50 psig
Operating Pressure 5-40 psig
Powder Capacity 181 kg (400 lb)
Powder Flow 15-100 lb/h (7-45 kg/h)
Relief Pressure 45 psig
Type Manual