ARCALOY 347-16

ARCALOY 347-16

How to order


Specifications

Approvals

ASME II SFA A5.4
E347-16
ASME IX F No. 5

Classifications

AWS A5.4
E347-16

Typical Mechanical Properties

Elongation in 2" 35 %
Tensile Strength As Welded 655 MPa (95 ksi)

Weld Metal Analysis

C 0.05 %
Mn 1.80 %

View full specs

Add to shopping list


Features

  • Arcaloy 347 electrodes are especially designed for welding types 347 and 321 alloys. This chromium-nickel alloy is used where conditions of service are such as to require maximum resistance to corrosion. Type 347 alloy was developed to prevent carbide precipitation.

Industries

  • Industrial and General Fabrication
  • Petrochemical
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications

Approvals

ASME II SFA A5.4
E347-16
ASME IX F No. 5

Classifications

AWS A5.4
E347-16

Typical Mechanical Properties

Elongation in 2" 35 %
Tensile Strength As Welded 655 MPa (95 ksi)

Weld Metal Analysis

C 0.05 %
Mn 1.80 %

View full specs

x

Inquire about the ARCALOY 347-16


×

Find the Closest Distributor

x

Find the Closest Distributor