ARCALOY 316/316H-16

ARCALOY 316/316H-16

Arcaloy 316/316H-16 should be used in applications where Type 316 stainless steel needs improved high temperature. In some cases an E16-8-2 filler metal should be used. It can also be used to weld Type 316 stainless steel for ambient temperature service.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 85 ksi 65 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.60 %2.30 %0.20 %0.05 %0.40 %5.5 FN %12 %19 %

Approvals: ABS, AWS A5.4: E316/316H-16, QPL MIL-E-22200/2, MIL-316-16
Classifications: AWS A5.4, E316/316H-16