ARCALOY 316LF5-16

ARCALOY 316LF5-16

Arcaloy 316LF5-16 is an E316L-16 electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. It can be used to weld Type 304L stainless steel where the presence of molybdenum is not detrimental.

Where To Buy


Industries

  • Petrochemical
  • Industrial and General Fabrication
  • Chemical Industry
  • Food and Beverage

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 83 ksi 65 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFerriteNiCr
1.50 %2.50 %0.20 %0.03 %0.40 %6 FN %12 %19 %

Approvals: CWB CSA W48; E316L-16; QPL MIL-E-22200/2; MIL-316L-16
Classifications: AWS A5.4; E316-16/E316L-16

Approvals are based on factory location. Please contact ESAB for more information.