ARCALOY 316LF5-16

ARCALOY 316LF5-16

Arcaloy 316LF5-16 is an E316L-16 electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. It can be used to weld Type 304L stainless steel where the presence of molybdenum is not detrimental.

Where To Buy


Industries

  • Chemical Industry
  • Food and Beverage
  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 83 ksi 65 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.50 %2.50 %0.20 %0.03 %0.40 %6 FN %12 %19 %

Approvals: CWB CSA W48, E316L-16, QPL MIL-E-22200/2, MIL-316L-16
Classifications: AWS A5.4, E316-16/E316L-16