Previous Next

ESAB

ARCALOY 316LF5-15

ARCALOY 316LF5-15

Arcaloy 316LF-15 is a 316L electrode designed to give a weld deposit with a minimum ferrite number of 5 FN. Carbon content is 0.04% maximum and can be used to weld Type 304L stainless steal where the presence of molybdenum is not detrimental.

Where To Buy


Industries

  • Chemical Industry
  • Food and Beverage
  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 81 ksi 62 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.50 %2.40 %0.20 %0.03 %0.50 %6 FN %12 %19 %

Approvals: QPL-22200/2, MIL-316L-15
Classifications: AWS A5.4, E316-15/E316L-15

Approvals are based on factory location. Please contact ESAB for more information.