ESAB

Shield-Bright 2507

Shield-Bright 2507

Shield-Bright 2507 is an all-position stainless steel cored wire designed for welding duplex stainless steel resulting in beautiful beads with excellent slag removal. It can deposit metal of 25% Cr-9% Ni-3.5% Mo-0.25% N. Shield-Bright 2507 is used in duplex stainless steels such as UNS S32520, S32550, S32750, S32760, S32900, JIS 329J4L.

Where To Buy


Welding Process

  • FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Elongation Tensile Strength Yield Strength
28 % 125 ksi 91 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoSCSiFerrite FNNiNCr
100% CO2
PMnMoSCSiFerrite FNNiNCr
0.010 %1.10 %3.75 %0.008 %0.03 %0.55 %40-65 %9.5 %0.22 %25.0 %