Cryo-Shield 316L

Cryo-Shield 316L

Cryo-Shield 316L is all position flux cored wire adaptable to a variety of shop and field erection applications. Designed for cryogenic applications where good weld metal toughness is required. Cryo-Shield 316L was developed for the welding of type 316, 316L austenitic stainless steels for the low temperatures. It contains molybdenum which resists pitting corrosion induced by sulphuric and sulphurous acids, chlorides and cellulose solutions. Cryo-Shield 316L was designed titania based slag system with excellent slag removal so they can have high welding speeds because of possible welding in all position in high current area.

Where To Buy


Welding Process

  • FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Elongation Tensile Strength Yield Strength
50 % 77 ksi 57 ksi

Typical Charpy V-Notch Properties

100% CO2
Impact Value Testing Temperature
29.5 ft-lb -321 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoSCSiFerrite FNNiCr
100% CO2
PMnMoSCSiFerrite FNNiCr
0.025 %1.50 %2.20 %0.008 %0.026 %0.70 %3-8 %12.4 %17.5 %

Approvals: JIS; NK; LR; BV; DNV; KR
Classifications: JIS Z3323; TS316L-FB1; AWS A5.22; E316LT1-1(4)