Cryo-Shield 308L

Cryo-Shield 308L

Cryo-Shield 308L is an all-position flux cored wire adaptable to a variety of shop and field erection applications. Designed for cryogenic applications where good weld metal toughness is required. Applications include cryogenic vessel fabrication and process piping repair. Cryo-Shield 308L was developed for the welding of types 304 & 304L stainless steels for the low temperature service, even down to liquid helium temperatures. This is done by controlling the composition and the ferrite content to give good toughness at temperatures of -321oF (-196oC) and lower. Cryo-Shield 308L was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

Where To Buy


Welding Process

  • FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Elongation Tensile Strength Yield Strength
59 % 80 ksi 53 ksi

Typical Charpy V-Notch Properties

100% CO2
Impact Value Testing Temperature
30 ft-lb -321 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiFerrite FNNiCr
100% CO2
PMnSCSiFerrite FNNiCr
0.027 %1.43 %0.010 %0.024 %0.67 %Max 8 %10.0 %18.50 %

Approvals: JIS; NK; LR; KR; DNV; BV
Classifications: JIS Z3323; TS308L-FB1; AWS A5.22; E308LT1-1(4)

Approvals are based on factory location. Please contact ESAB for more information.