ESAB

OK Tigrod NiCrMo-4


OK Tigrod NiCrMo-4 is a corrosion and heat resistant, nickel-chromium rod for TIG welding of high alloyed steel, heat resistant steel, corrosion resistant steel, 9Ni steels and similar steels with high notch toughness at low temperatures. Good resistance to stress corrosion.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnMoCSiWNiCrFe
0.45 %16.1 %0.01 %0.05 %3.5 %Bal. %15.5 %5.8 %

Classifications: SFA/AWS A5.14, ERNiCrMo-4, Wire Electrode, EN ISO 18274, S Ni 6276 (NiCr15Mo16Fe6W4), Wire Electrode