Previous Next

ESAB

OK Autrod 2307


A continous, solid, corrosion-resistent duplex wire for welding austenitic-ferritic stainless alloys of the 21% Cr-1% Ni or 23% Cr-4% Ni type. OK Autrod 2307 is overalloyed in Ni to ensure a correct Ferrite balance in the weld metal. Lean duplex types are used for civil engineering, storage tanks, containers, etc. These steels have in general medium corrosion resistance and good strength properties. The welding should be done as for ordinary austenitic steels, but high amperages should be avoided and interpass temperature should be maximum 150°C.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
32 % 106 ksi 81 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
118 ft-lb 68 °F
44 ft-lb -76 °F

Typical Weld Metal Analysis %

MnMoCuCSiNiNCr
1.4 %3.20 %0.2 %0.01 %0.5 %7.1 %0.15 %23.2 %

Approvals: CE, EN 13479
Classifications: EN ISO 14343-A, G 23 7 N L, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.