This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

Shield-Bright 309L

Shield-Bright 309L

Shield-Bright 309L is a rutile cored wire designed for the all-positional welding, except vertical down, of stainless steels to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels with Ar/15-25%CO2 or CO2 shielding gas.

Where To Buy


Specifications


Typical Tensile Properties

75% Ar - 25% CO2 As welded
Elongation Tensile Strength Yield Strength
35 % 87 ksi 70 ksi
100% CO2 As welded
Elongation Tensile Strength Yield Strength
51 % 78 ksi 57 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 40.5 ft-lb -20 °F
As Welded 13 ft-lb -321 °F

Typical Weld Metal Analysis %

PMnSCSiNiCr
0.024 %1.30 %0.007 %0.030 %0.90 %12.5 %23.5 % 0.024 %1.10 %0.007 %0.029 %0.80 %12.4 %23.1 %

Approvals: ABS-AWS A5.22, E309LT1-1, ASME II SFA 5.22 E309LT1-1/T1-4, ASME IX F No. 6, AWS A5.22, E309LT1-1/T1-4, CWB, AWS A5.22 E309LT1-1, E309LT1-4, G.L.- AWS A5.22, E309LT1-4, MIL-STD-1689 APPLICATIONS-NAVY, TUV
Classifications: AWS A5.22, E309T1-1/T1-4, A5.22, E309LT1-1/T1-4

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Cr Ni
Welding Current: DC+