Shield-Bright 308L

Shield-Bright 308L

Shield-Bright 308L was developed for welding type 304L stainless steel and can also be used for welding types 301, 302, and 304 steels. It may also be used for welding types 321 and 347 if the service conditions do not exceed an approximate of 750°F (399°C).

Where To Buy


Specifications


Typical Tensile Properties

75% Ar - 25% CO2 As welded
Elongation Tensile Strength Yield Strength
44 % 84 ksi 59.5 ksi
100% CO2 As welded
Elongation Tensile Strength Yield Strength
61 % 82 ksi 54 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 44 ft-lb -20 °F
As Welded 22 ft-lb -321 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnSCSiNiCr
0.025 %1.20 %0.007 %0.030 %0.90 %10.1 %19.3 %
100% CO2
PMnSCSiNiCr
0.025 %1.10 %0.007 %0.025 %0.70 %10.0 %19.1 %

Approvals: CWB, AWS A5.22 E308LT1-1, E308LT1-4, VdTÜV, 04832 (M20,M21), LR, 304L (C1), KR, RW308LG (C) (C1), DNV, NV 308L (C1), ClassNK, KW308LG(C) (C1), CCS, 308L (C1), ABS, E308LT1-1 (C1), CE EN, 13479
Classifications: EN ISO 17633-A, T 19 9 L P M21 2, EN ISO 17633-A, T 19 9 L P C1 2, KS D 3612, YF 308LC, JIS Z 3323, TS308L-FB1, SFA/AWS A5.22, E308LT1-1, SFA/AWS A5.22, E308LT1-4

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Cr Ni
Welding Current: DC+