Shield-Bright 308L Xtra

Shield-Bright 308L Xtra

Shield-Bright 308L X-tra was designed for welding type 304L stainless steel but can be used for types 301, 302,and 304 steels. It may also be used successfully for welding of types 321 and 347 stainless steel. Service conditions should not exceed an approximate of 750°F (399°C). Shield-Bright 308L X-tra was designed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.

Where To Buy


Specifications


Typical Tensile Properties

75% Ar - 25% CO2 As welded
Elongation Tensile Strength Yield Strength
40 % 84 ksi 59.5 ksi
100% CO2 As welded
Elongation Tensile Strength Yield Strength
55 % 80 ksi 59 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 29.5 ft-lb -20 °F
As Welded 18 ft-lb -321 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnSCSiNiCr
0.020 %1.40 %0.004 %0.022 %0.90 %9.9 %19.6 %
100% CO2
PMnSCSiNiCr
0.020 %1.30 %0.004 %0.030 %0.48 %9.8 %19.4 %

Approvals: VdTÜV, 06611, LR, 304L S (C1), KR, RW308LG(C) (C1), DNV, 308L (C1), CWB, AWS A5.22 E308LT0-1, E308LT0-4, BV, 308L (M21), ABS, E308LT0-1 (C1), CE EN, 13479
Classifications: EN ISO 17633-A, T 19 9 L R M21 3, EN ISO 17633-A, T 19 9 L R C1 3, KS D 3612, YF 308LC - KR, JIS Z 3323, TS308L-FB0 - KR, SFA/AWS A5.22, E308LT0-4, SFA/AWS A5.22, E308LT0-1

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Cr Ni
Welding Current: DC+