OK Autrod 430LNb

A continous ferritic stainless solid wire with low carbon content, 18 % Cr and stabilized with Nb, for welding similar and matching steels. OK Autrod 430LNb (W) is developed and designed for the automotive industry and used for production of exhaust systems. The wire should be used when there is a need for good resistance to corrosion and thermal fatigue. The OK Autrod 430LNb (W) is a new version of OK Autrod 430LNb, with restricted Nb limits.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
26 % 61 ksi 40 ksi

Typical Weld Metal Analysis %

MnMoCuCNbSiNiCr
0.5 %0.06 %0.10 %0.01 %0.45 %0.5 %0.2 %18.5 %

Classifications: EN ISO 14343-A, G 18 L Nb, Wire Electrode, Werkstoffnummer, ~1.4511, Wire Electrode

Alloy Type: 18 % Cr - 0.5 % Nb