OK Autrod 309Si

OK Autrod 309Si

A continuous solid corrosion resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni, high C types. OK Autrod 309Si has a good general corrosion resistance. The higher silicon content improves the welding properties such as wetting. When used for joining dissimilar materials the corrosion resistance is of secondary importance.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
36 % 90 ksi 64 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
74 ft-lb 68 °F
59 ft-lb -76 °F
44 ft-lb -166 °F

Typical Weld Metal Analysis %

MnMoCuCSiFerrite FNNiCr
1.8 %0.20 %0.15 %0.08 %0.9 %5 %12.7 %23.3 %

Classifications: EN ISO 14343-A, G 22 12 H, Wire Electrode, SFA/AWS A5.9, ER309Si, Wire Electrode, Werkstoffnummer, ~1.4829, Wire Electrode

Alloy Type: Austenitic (with approx. 10 % ferrite) 23 % Cr - 13 % Ni - High Si