OK Autrod 308L SAW


A continuous, solid, corrosion-resistant, chromium-nickel wire. OK Autrod 308L has good general corrosion resistance. The alloy has a low carbon content which makes it particularly suitable for applications where there is a risk of intergranular corrosion. OK Autrod 308L is widely used in the chemical and food-processing industries, as well as for pipes, tubes and boilers and can be used in combination with OK Flux 10.93, OK Flux 10.94 or OK Flux 10.95.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnCSiNiNCr
1.9 %0.02 %0.4 %9.8 %0.05 %19.8 %

Approvals: CE; EN 13479; DB; 52.039.15; NAKS/HAKC; 3.2-4.0 mm; VdTÜV; 12101
Classifications: EN ISO 14343-A; S 19 9 L; Wire Electrode; SFA/AWS A5.9; ER308L; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 10 % ferrite) 19% Cr - 9% Ni - Low C