Previous Next

ESAB

OK Autrod 2509


A continous solid corrosion resisting “Super Duplex” wire for welding of austenitic-ferritic stainless alloys of 25% Cr, 10% Ni, 4% Mo, low C types. OK Autrod 2509 has a high intergranular corrosion resistance and pitting. The alloy is widely used in applications were corrosion resistance is of utmost importance. Pulp and paper industry, offshore and gas industry are areas of interest. OK Autrod 2509 can be used in combination with OK Flux 10.93 or OK Flux 10.94.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCSiNiNCr
0.4 %3.9 %0.01 %0.4 %9.4 %0.24 %25.2 %

Approvals: CE, EN 13479, VdTÜV, 12101
Classifications: EN ISO 14343-A, S 25 9 4 N L, Wire Electrode, SFA/AWS A5.9, ER2594, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic-ferritic (25% Cr - 10% Ni - 4% Mo - Low C)