OK Autrod 2209


A duplex austenitic-ferritic stainless welding strip designed for submerged arc cladding. It is used with OK Flux 10.05 to produce a 2209 duplex stainless steel type of weld deposit.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnMoCSiNiNCr
1.5 %3.2 %0.01 %0.5 %8.5 %0.17 %22.7 %

Approvals: CE, EN 13479, VdTÜV, 12101, NAKS/HAKC, 3.2-4.0mm, CZ
Classifications: EN ISO 14343-A, S 22 9 3 N L, Wire Electrode, SFA/AWS A5.9, ER2209, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic-ferritic (22.5 % Cr - 8 % Ni - 3 % Mo - Low C)