A continuous solid corrosion resisting chromium-nickel-molybdenum-copper wire for welding of austenitic stainless alloys of 20% Cr, 25% Ni, 5% Mo, 1,5% Cu, low C types. OK Autrod 385 weld metal has a good resistance to stress corrosion and intergranular corrosion and shows a very good resistance to attack in non-oxidizing acids. The resistance and crevice corrosion is better than for ordinary 18% Cr, 8% Ni, Mo steels. The alloy is widely used in many applications related to the process industry. OK Autrod 385 can be used in combination with OK Flux 10.93.

Where To Buy


Typical Weld Metal Analysis %

1.7 %4.4 %1.5 %0.01 %0.4 %25.0 %0.05 %20.0 %

Approvals: VdTÜV, 12101
Classifications: EN ISO 14343-A, S 20 25 5 Cu L, Wire Electrode, SFA/AWS A5.9, ER385, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.

Alloy Type: Fully austenitic (20 % Cr - 25 % Ni - 5 % Mo - 1.5 % Cu - Low C)