OK Autrod 318


OK Autrod 318 is an extra low carbon, stainless wire for the submerged arc welding of corrosion-resistant steels of the 18Cr12Ni3Mo type, such as AlSi 316 and 316L or somewhat lower alloyed types. OK Autrod 318 can be used in combination with OK Flux 10.93.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCNbSiFN WRC-92NiNCr
1.8 %2.6 %0.04 %0.7 %0.4 %11 %11.5 %0.04 %18.9 %

Approvals: CE, EN 13479, DB, 52.039.11, NAKS/HAKC, 4.0mm, VdTÜV, 12101
Classifications: EN ISO 14343-A, S 19 12 3 Nb, Wire Electrode, SFA/AWS A5.9, ER318, Wire Electrode