OK Tigrod 5554

OK Tigrod 5554

OK Tigrod 5554 is a solid aluminium rod with a content of 2.7% Mg. It is recommended for the welding of AlMg alloys like 5454. Typical applications include chemical storage tanks, automotive components like wheels and frame sections. The weld metal is not sensitive to stress corrosion cracking at elevated temperatures.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
17 % 33 ksi 16 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCuZnTiSiMgAlCrFe
0.7 %0.01 %0.01 %0.15 %0.1 %2.7 %96 %0.1 %0.1 %

Approvals: CWB; A5.10/A5.10:2012 ER5554
Classifications: SFA/AWS A5.10; R5554; Wire Electrode; EN ISO 18273; S Al 5554 (AlMg2,7Mn); Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMg 5