OK Tigrod 1100

OK Tigrod 1100

OK Tigrod 1100 is highly resistant to chemical attack and weathering. It is a relatively soft alloy that is very formable and it is used extensively in thin-gauge and foil products. It has good welding characteristics. One desirable characteristic of the alloy is the bright finish obtained by anodising. Non-heat treatable.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 35 % 11 ksi 4 ksi

Typical Weld Metal Analysis %

CuBeZnSi+Fe
0.07 %0.0001 %0.01 %0.55 %

Approvals: CWB, AWS A5.10/A5.10M:2012 (ER1100)
Classifications: SFA/AWS A5.10, R1100, Wire Electrode, EN ISO 18273, S Al 1100 (Al99,0Cu), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Al