ESAB

OK Tigrod 1070

OK Tigrod 1070

OK Tigrod 1070 is highly resistant to chemical attack and weathering. It is a relatively soft alloy that is very formable and it is used extensively in thin-gauge and foil products. It has good welding characteristics. One characteristic feature of the alloy is the bright finish obtained by anodising. Non-heat treatable.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 33 % 11 ksi 5 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCuSiVAlFe
0.01 %0.01 %0.02 %0.01 %99.80 %0.13 %