OK Tigrod 347


Bare, corrosion-resistant, chromium-nickel rods for welding stabilised austenitic chromium-nickel alloys of the 18% Cr-8% Ni type. The rods are stabilised with niobium, which provides good resistance to the intergranular corrosion of the weld metal. Due to the niobium content, this alloy is recommended for use at higher temperatures.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
35 % 95 ksi 74 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
96 ft-lb 68 °F

Typical Weld Metal Analysis %

MnMoCuCNbSiFerrite FNNiCr
1.4 %0.10 %0.05 %0.04 %0.50 %0.4 %7 %9.5 %19.3 %

Approvals: NAKS/HAKC, 2.4mm
Classifications: EN ISO 14343-A, W 19 9 Nb, Wire Electrode, SFA/AWS A5.9, ER347, Wire Electrode, Werkstoffnummer, ~1.4551, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Nb