OK Tigrod 2509


Bare, corrosion-resistant, “Super Duplex’’ rods for welding austenitic-ferritic stainless alloys of the 25% Cr, 7% Ni, 4% Mo, low C types. OK Autrod 2509 has high intergranular-corrosion, pitting and stress-corrosion resistance. The alloy is widely used in applications where corrosion resistance is of the utmost importance. The pulp and paper industry, offshore and gas industry are areas of interest.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
37 % 121 ksi 96 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
147.5 ft-lb -76 °F
133 ft-lb -58 °F

Typical Weld Metal Analysis %

MnMoCuCSiWNiCr
0.4 %4.0 %< 0.3 %< 0.02 %0.4 %< 1.0 %9.8 %25.0 %

Approvals: UDT DIN 8556, VdTÜV 06593 (IT)
Classifications: EN ISO 14343, W 25 9 4 NL

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic-ferritic (25 % Cr - 10 % Ni - 4 % Mo - Low C)