ESAB

OK Tigrod 410NiMo


Bare welding rods of the 420NiMo type alloyed with 13% Cr, 4.5% Ni and 0.5% Mo. This alloy is used for welding similar composition martensitic and martensitic-ferritic steels in different applications, such as hydroturbines.

Where To Buy


Specifications


Typical Tensile Properties

Stress relieved
Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
17 % 1112 °F 2 hr 145 ksi 135 ksi
22 % 1112 °F 8 hr 126 ksi 112 ksi

Typical Charpy V-Notch Properties

Stress relieved
Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
88.5 ft-lb 1112 °F 2 hr 32 °F
88.5 ft-lb 1112 °F 2 hr -76 °F
129 ft-lb 1112 °F 8 hr 32 °F
122 ft-lb 1112 °F 8 hr -76 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
0.5 %0.6 %0.1 %0.02 %0.4 %4.2 %12.4 %

Classifications: EN ISO 14343-A; W 13 4; Wire Electrode

Alloy Type: Martensitic-ferritic (13 % Cr - 4.5 % Ni - 0.5 % Mo)