OK Tigrod 310


Bare, corrosion-resistant, chromium-nickel welding rod for welding heat-resistant austenitic steels of the 25Cr-20Ni type. The wire has a high Cr content and provides good oxidation resistance at high temperatures. Common applications include industrial furnaces and boiler parts, as well as heat exchangers.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
43 % 85.5 ksi 56.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
129 ft-lb 68 °F
44 ft-lb -321 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
1.6 %0.10 %0.05 %0.10 %0.4 %20.7 %25.8 %

Classifications: EN ISO 14343-A; W 25 20; Wire Electrode; SFA/AWS A5.9; ER310; Wire Electrode