OK Tigrod 309L


Bare corrosion resisting chromium-nickel welding rod for welding of similar steels of 24% Cr, 13% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld. OK Tigrod 309L has a good general corrosion resistance. When used for joining dissimilar materials the corrosion resistance is of secondary importance.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 85.5 ksi 62 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
118 ft-lb 68 °F
96 ft-lb -76 °F
66 ft-lb -166 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFN WRC-92NiNCr
1.8 %0.10 %0.08 %0.02 %0.4 %9 %13.4 %0.05 %23.2 %

Approvals: CE; EN 13479; CWB; ER309L; NAKS/HAKC; 1.6MM; VdTÜV; 10021
Classifications: EN ISO 14343-A; W 23 12 L; Wire Electrode; SFA/AWS A5.9; ER309L; Wire Electrode; Werkstoffnummer; ~1.4332; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 10 % ferrite) 24 % Cr - 13 % Ni - Low C