OK Tigrod 309LSi

Bare, corrosion-resistant, chromium-nickel welding rod for welding steels with similar composition, wrought and cast steels of the 23% Cr-12% Ni types. The alloy is also used for welding buffer layers on CMn steels and for welding dissimilar joints. When using the wire for buffer layers and dissimilar joints, it is necessary to control the dilution of the weld. OK Tigrod 309LSi has good general corrosion resistance. The higher silicon content improves the welding properties such as wetting.

Where To Buy


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
32 % 92 ksi 69 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
111 ft-lb 68 °F
111 ft-lb 32 °F
111 ft-lb -76 °F
96 ft-lb -166 °F

Typical Weld Metal Analysis %

MnMoCuCSiFerrite FNNiCr
1.7 %0.15 %0.12 %0.02 %0.9 %9 %13.5 %23.4 %

Approvals: CE, EN 13479, DB, 43.039.17, NAKS/HAKC, 2.4mm, VdTÜV, 12489
Classifications: EN ISO 14343-A, W 23 12 L Si, Wire Electrode, SFA/AWS A5.9, ER309LSi, Wire Electrode, Werkstoffnummer, ~1.4332, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.

Alloy Type: Austenitic (with approx. 8 % ferrite) 24 % Cr - 13 % Ni - Low C