ESAB

OK Tigrod 316LSi


Bare, corrosion-resistant, chromium-nickel-molybdenum rods for welding austenitic stainless alloys of the 18% Cr-8% Ni and 18% Cr-10% Ni-3% Mo types. OK Tigrod 316LSi has good general corrosion resistance, particularly to corrosion in acid and chlorinated environments. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The higher silicon content improves the welding properties such as wetting. The alloy is widely used in the chemical and food-processing industries, as well as in shipbuilding and various types of architectural structure.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
33 % 91 ksi 72.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
129 ft-lb 68 °F
81 ft-lb -166 °F
66 ft-lb -321 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFerrite FNNiCr
1.8 %2.60 %0.12 %0.01 %0.9 %7 %12.2 %18.4 %

Approvals: BV; 316L BT; CE; EN 13479; DB; 43.039.06; DNV; 316L (-196°C); GL; 4429 (I1); NAKS/HAKC; 2.0MM-2.4MM; VdTÜV; 05336
Classifications: EN ISO 14343-A; W 19 12 3 L Si; Wire Electrode; SFA/AWS A5.9; ER316LSi; Wire Electrode; Werkstoffnummer; ~1.4430; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 8 % ferrite) 19% Cr - 12% Ni - 3% Mo - Low C- High Si