OK Tigrod 316L

Bare corrosion resisting chromium-nickel-molybdenium welding rods for welding of austenitic stainless alloys of 18% Cr - 8% Ni and 18% Cr - 10% Ni - 3% Mo-types. OK Tigrod 316L has a good general corrosion resistance, particularly against corrosion in acid and chlorinated environments. The alloy has a low carbon content which makes it particularly recommended where there is a risk of intergraular corrosion. The alloy is widely used in the chemical and food processing industries as well as in shipbuilding and various types of architectural structures.

Where To Buy


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
32 % 87 ksi 68 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
129 ft-lb 68 °F
96 ft-lb -76 °F
88.5 ft-lb -166 °F
55 ft-lb -321 °F

Typical Weld Metal Analysis %

1.7 %2.6 %0.01 %0.4 %7 %12.0 %0.04 %18.2 %

Approvals: ABS, ER 316L, BV, 316L BT, CE, EN 13479, CWB, ER316L, DNV-GL, VL 316 L (I1), NAKS/HAKC, 2.0-3.2 mm, VdTÜV, 04270
Classifications: EN ISO 14343-A, W 19 12 3 L, Wire Electrode, SFA/AWS A5.9, ER316L, Wire Electrode, Werkstoffnummer, ~1.4430, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.

Alloy Type: Austenitic (with approx. 10 % ferrite) 19% Cr - 12% Ni - 3% Mo - Low C