OK Tigrod 308H


Bare, corrosion-resistant, chromium-nickel rods for welding austenic chromium-nickel alloys of the18% Cr-8% Ni type. OK Tigrod 308H has good general corrosion resistance. The alloy has a high carbon content, which makes it suitable for applications at higher temperatures. The alloy is used in the chemical and petrochemical industries for the welding of tubes, cyclones and boilers.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
30 % 80 ksi 51 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
1.9 %0.15 %0.1 %0.05 %0.5 %9.2 %19.8 %

Classifications: EN ISO 14343-A; W 19 9 H; Wire Electrode; SFA/AWS A5.9; ER308H; Wire Electrode

Alloy Type: Austenitic 19% Cr - 9% Ni - High C