OK Tigrod 308LSi


Bare, corrosion-resistant, chromium-nickel rods for welding austenitic chromium-nickel alloys of the18% Cr-8% Ni type. OK Tigrod 308LSi has good general corrosion resistance. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The higher silicon content improves the welding properties such as wetting. The alloy is widely used in the chemical and food-processing industries, as well as for pipes, tubes and boilers.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
37 % 91 ksi 70 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
125 ft-lb 68 °F
111 ft-lb -76 °F
103 ft-lb -166 °F
55 ft-lb -321 °F

Typical Weld Metal Analysis %

MnMoCuCSiFerrite FNNiCr
1.8 %0.15 %0.10 %0.01 %0.9 %9 %10.5 %19.9 %

Approvals: BV, 308L BT, CE, EN 13479, DB, 43.039.11, DNV, 308L M, NAKS/HAKC, 2.0MM-3.2MM, VdTÜV, 05335
Classifications: EN ISO 14343-A, W 19 9 L Si, Wire Electrode, SFA/AWS A5.9, ER308LSi, Wire Electrode, Werkstoffnummer, ~1.4316, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Low C