A ferritic, stainless, solid wire with a content of 18% Cr and stabilised with 0.5% Ti for welding similar and matching steels. The alloy is also used for cladding on unalloyed and low-alloyed steels. OK Autrod 430Ti is also widely used in the automotive industry for the welding of manifolds, catalytic converters and exhaust pipes.

Add to shopping list


Specifications


Typical Tensile Properties

Stress relieved
Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
24 % 1436 °F 0.5 hr 87 ksi 56.5 ksi
28 % 1436 °F 0.5 hr 84 ksi 55 ksi

Typical Weld Metal Analysis %

MnMoCuCTiSiNiCr
0.5 %0.05 %0.10 %0.07 %0.400 %0.9 %0.3 %17.6 %

Approvals: CE, EN 13479
Classifications: EN ISO 14343-A, G Z 17 Ti, Wire Electrode, Werkstoffnummer, 1.4502, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: 18 % Cr - 0.5 % Ti