This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

OK Autrod 410NiMo


A continuous, solid welding wire of the 12% Cr, 4.5% Ni, 0.5% Mo type. OK Autrod 410NiMo is used for welding similar martentsitic and martensitic-ferritic steels in different applications, such as hydro turbines.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength Stress Relieved Temperature Stress Relieved Testing Time
13 % 152 ksi 125 ksi - -
Stress relieved
Elongation Tensile Strength Yield Strength Stress Relieved Temperature Stress Relieved Testing Time
17 % 130.5 ksi 123 ksi 1112 °F 2 hr
20 % 123 ksi 109 ksi 1112 °F 8 hr

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
26 ft-lb 32 °F - -
22 ft-lb -4 °F - -
Stress relieved
Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
52 ft-lb 32 °F 1112 °F 2 hr
40.5 ft-lb -4 °F 1112 °F 2 hr
55 ft-lb 32 °F 1112 °F 8 hr
55 ft-lb -4 °F 1112 °F 8 hr

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
0.5 %0.6 %0.1 %0.02 %0.4 %4.2 %12.4 %

Classifications: EN ISO 14343-A; G 13 4; Wire Electrode

Alloy Type: Martensitic-ferritic (12 % Cr - 4.5 % Ni - 0.5 % Mo)