Previous Next

ESAB

OK Autrod 312


A continuous, solid, corrosion-resistant, chromium-nickel wire for welding stainless steels of the 29% Cr, 9% Ni types. OK Autrod 312 has good oxidation resistance at high temperatures due to its high content of Cr. The alloy is widely used for joining dissimilar steels, especially if one of the components is fully austenitic, and steels that are difficult to weld, i.e. machine components, tools and austenitic-manganese steels.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
20 % 112 ksi 88.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
67 ft-lb 68 °F

Typical Weld Metal Analysis %

MnMoCuCSiNiCr
1.6 %0.20 %0.14 %0.10 %0.4 %8.8 %30.7 %

Classifications: EN ISO 14343-A, G 29 9, Wire Electrode, SFA/AWS A5.9, ER312, Wire Electrode