OK Autrod 310


A continuous, solid ,corrosion-resistant, chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. OK Autrod 310 has good general oxidation resistance, especially at high temperatures, due to its high Cr content. The alloy is fully austenitic and is therefore sensitive to hot cracking. Common applications include industrial furnaces and boiler parts, as well as heat exchangers.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
43 % 85.5 ksi 56.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
129 ft-lb 68 °F
44 ft-lb -321 °F

Typical Weld Metal Analysis %

MnCSiNiCr
1.6 %0.10 %0.4 %20.7 %25.8 %

Approvals: CE, EN 13479
Classifications: EN ISO 14343-A, G 25 20, Wire Electrode, SFA/AWS A5.9, ER310, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Fully austenitic (25 % Cr - 20 % Ni)