ESAB

OK Autrod 309LSi


A continous solid corrosion resistant chromium-nickel wire for welding of similar steels, wrought and cast steels of 23% Cr-12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld. OK Autrod 309LSi has a good general corrosion resistance. The higher silicon content improves the welding properties, such as wetting.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
41 % 87 ksi 64 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
118 ft-lb 68 °F
96 ft-lb -76 °F
66 ft-lb -166 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFerrite FNNiCr
1.7 %0.15 %0.12 %0.02 %0.9 %9 %13.5 %23.4 %

Approvals: CE; EN 13479; CWB; ER309LSi; DB; 43.039.16; NAKS/HAKC; 1.0MM-1.2MM; VdTÜV; 10020
Classifications: EN ISO 14343-A; G 23 12 L Si; Wire Electrode; SFA/AWS A5.9; ER309LSi; Wire Electrode; Werkstoffnummer; ~1.4332; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 8 % ferrite) 24 % Cr - 13 % Ni - Low C