OK Autrod 316LSi


A continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding austenitic stainless alloys of the 18% Cr -8% Ni and 18% Cr -10% Ni -3% Mo types. OK Autrod 316LSi has good general corrosion resistance; in particular, the alloy has very good resistance to corrosion in acid and chlorinated environments. The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. The higher silicon content improves the welding properties such as wetting. The alloy is widely used in the chemical and food processing industries, as well as in shipbuilding and various types of architectural structure.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
37 % 81 ksi 58 ksi
Tested at 350°C (662°F). As welded
Elongation Tensile Strength Yield Strength
26 % 64 ksi 49 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
88.5 ft-lb 68 °F
70 ft-lb -76 °F
52 ft-lb -166 °F
33 ft-lb -321 °F

Typical Weld Metal Analysis %

MnMoCuCSiFerrite FNNiCr
1.8 %2.60 %0.12 %0.01 %0.9 %7 %12.2 %18.4 %

Approvals: CE, EN 13479, CWB, ER316LSi, DB, 43.039.05, DNV, NV 316L (M13), VdTÜV, 04268, NAKS/HAKC, 1.0MM-1.2MM
Classifications: EN ISO 14343-A, G 19 12 3 L Si, Wire Electrode, SFA/AWS A5.9, ER316LSi, Wire Electrode, Werkstoffnummer, ~1.4430, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (with approx. 8 % ferrite) 19% Cr - 12% Ni - 3% Mo - Low C - High Si