OK Autrod 308H


A continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18% Cr-8% Ni type. OK Autrod 308H has good general corrosion resistance. The alloy has a high carbon content, making it suitable for applications used at higher temperatures. The alloy is used in chemical and petrochemical plants for the welding of pipes, cyclones and boilers.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnMoCuCSiNiCr
1.9 %0.15 %0.1 %0.05 %0.5 %9.2 %19.8 %

Classifications: EN ISO 14343-A, G 19 9 H, Wire Electrode, SFA/AWS A5.9, ER308H, Wire Electrode

Alloy Type: Austenitic 19% Cr - 9% Ni - High C