OK Autrod 317L


A continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding austenitic stainless alloys of the 19% Cr, 13% Ni, 3% Mo types. OK Autrod 317L has good resistance to general corrosion and pitting due to its high content of molybdenum. The alloy has a low carbon content which makes it particularly recommended where there is a risk of intergranular corrosion. The alloy is used in severe corrosion conditions, such as in the petrochemical, pulp and paper industries.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
45 % 87 ksi 56.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
99.5 ft-lb 68 °F
40.5 ft-lb -321 °F

Typical Weld Metal Analysis %

MnMoCuCSiFN WRC-92NiNCr
1.4 %3.6 %0.05 %0.01 %0.4 %7 %13.6 %0.05 %18.9 %

Classifications: EN ISO 14343-A, G 18 15 3 L, Wire Electrode, SFA/AWS A5.9, ER317L, Wire Electrode

Alloy Type: Austenitic (with approx. 8 % ferrite)