Coreshield 8 is a self-shielded flux cored wire designed to weld critical structural applications while maintaining excellent arc characteristics and high welder appeal using DCEN polarity. Coreshield 8 is tested and certified to meet the new AWS D designation requirements, making this self-shielded wire an excellent choice for demand critical welds when the AWS D1.8 Seismic Supplement is utilized

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 24 % 82 ksi 67 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 30 ft-lb -20 °F
As Welded 65 ft-lb 40 °F

Typical Weld Metal Analysis %

PMnSCSiAl
0.010 %0.44 %0.003 %0.19 %0.15 %0.51 %

Approvals: DB, Seismic Certified "D", BV, LR, DNV-GL, ABS, CWB, CSA W48 E491T-8-H8
Classifications: ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T8-A2-CS3-H8, AWS A5.20, E71T-8 JD-H8

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Mn
Welding Current: DC-