Previous Next

ESAB

Tigrod 1450

Tigrod 1450

OK Tigrod 1450 is highly resistant to chemical attack and weathering. The alloy has a small addition of titanium, which has a grain-refining effect, which reduces cracking susceptibility. It has good welding characteristics. One characteristic feature of the alloy is the bright finishes obtained by anodising. Non-heat treatable.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 35 % 13 ksi 6 ksi

Typical Weld Metal Analysis %

MnCuZnTiSiAlFe
0.02 %0.01 %0.01 %0.12 %0.02 %99.8 %0.16 %

Classifications: EN ISO 18273, S Al 1450 (Al99,5Ti), Wire Electrode