OK Tigrod 5556A

OK Tigrod 5556A

Bare welding rod suitable for welding aluminium alloys with up to approx. 5% Mg that are not age hardenable and alloys where a higher tensile strength is required. The corrosion resistance in a marine atmosphere is very good.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 43 ksi 21 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 18 ft-lb 68 °F

Classifications: SFA/AWS A5.10; R5556; EN ISO 18273; S Al 5556A (AlMg5Mn)