ESAB

OK AristoRod 12.62


OK AristoRod 12.62 is a bare triple deoxidised ER70S-2 solid wire for the GMAW of non-alloyed steels, as used in general construction, pressure vessel fabrication and shipbuilding. It yields high-quality welds in semi-killed and rimmed steels, as well as with grades with various carbon contents. Added deoxidants, Al - Ti- Zr, make the wire also suitable for steels with a dirty or rusty surface, without sacrificing weld quality. OK AristoRod 12.62 is treated with ESAB’s unique Advanced Surface Characteristics (ASC) technology, taking MIG/MAG welding operations to new levels of performance and all-round efficiency, especially in robotic and mechanised welding. Characteristic features include excellent start properties; trouble-free feeding at high wire speeds and lengthy feed distances; a very stable arc at high welding currents; extremely low levels of spatter; low fume emission; reduced contact tip wear and improved protection against corrosion of the wire.

Where To Buy


Industries

  • Power Generation
  • Pipeline
  • Ship and Offshore Yards
  • Barges

Specifications


Typical Tensile Properties

80% Ar - 20% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 91 ksi 83 ksi

Typical Charpy V-Notch Properties

80% Ar - 20% CO2
Condition Impact Value Testing Temperature
As Welded 133 ft-lb -40 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCuMoSCVSiAlNiTi+ZrCr
0.008 %1.1 %0.05 %0.01 %0.009 %0.06 %0.01 %0.60 %0.12 %0.03 %0.13 %0.12 %

Classifications: SFA/AWS A5.18:; ER70S-2; EN ISO 14341-A:; G 2Ti; Wire Electrode

Alloy Type: Carbon-manganese steel (Mn/Si-alloyed)