Previous Next

ESAB

OK Band NiCr3


OK Band NiCr3 is a nickel-based strip for submerged arc strip cladding. Together with OK Flux 10.11, OK Flux 10.16 or OK Flux 10.17 it produces a weld overlay with good corrosion resistance and high temperature properties.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnCSiNiNb+TaCrFe
3.0 %< 0.1 %0.2 %≥67.0 %2.6 %20.0 %≤3.0 %

Approvals: VdTÜV, 12102
Classifications: SFA/AWS A5.14, EQNiCr-3, EN ISO 18274, B Ni 6082 (NiCr20Mn3Nb)