OK Autrod 16.38


A continuous solid corrosion resisting non-magnetic chromium-nickel-molybdenium wire for welding of stabilized and non-stabilized austenitic alloys of the same type as well as non magnetic steels. The alloy is corrosion resistant in seawater environment and has very good corrosion resistance to acids such as nitric acid. Excellent impact properties at low temperatures

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 87 ksi 58 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
66 ft-lb -76 °F
52 ft-lb -166 °F
29.5 ft-lb -321 °F

Typical Weld Metal Analysis %

MnMoCSiNiNCr
6.9 %3.0 %0.01 %0.4 %16.5 %0.18 %19.9 %

Classifications: EN ISO 14343-A, G 20 16 3 Mn L, Wire Electrode

Alloy Type: Austenitic (7 % Mn - 20 % Cr - 16 % Ni - 3 % Mo)