OK Tigrod 18.22

OK Tigrod 18.22 is suitable for welding aluminium alloys with a magnesium content of more than 3% where high strength is required. The alloy has a small addition of zirconium that has a fine graining effect that makes it less sensitive to hot cracking during solidification. Non-heat treatable.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 48 ksi 23 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 19 ft-lb 68 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCuTiSiZrMgAl
0.8 %0.03 %0.03 %0.06 %0.1 %5.8 %92.93 %